±¸ ºÐ |
YZ
(ZrO2+Y2O3) |
MZ
(ZrO2+MgO) |
Density(g/cc) ¹Ðµµ |
6.0ÀÌ»ó |
5.6ÀÌ»ó |
Load0.5KgHV1=9.807NVickers
Hardness(Gpa)ºñÄ¿½º°æµµ |
13.2 |
10.7 |
Bending Strength(MPa) ±ÁÈû°µµ |
1000 |
750 |
Compressive Strength(Mpa) ¾ÐÃà°µµ |
5690 |
- |
Fracture Toughness(MPa¡îM) |
7.5 |
7.0 |
Coefficient of Thermal Expansion
[40~400¡É] (x10-6) |
10.5 |
10 |
Coefficient of Thermal Expansion
[40~800¡É] (x10-6) |
11.0 |
10.5 |
Thermal Conductivity [20¡É] (¡É) |
3 |
3 |
Thermal Shock Resistance (¡É) |
250 |
450 |
Nireic Acid
(Weught Loss mg/cm2/day) |
0 |
- |
Sulphuric Acid
(Weught Loss mg/cm2/day) |
0.04 |
- |
Caustic Soda
(Weught Loss mg/cm2/day) |
0.08 |
- |